围压与料浆浓度对尾砂充填体峰后损伤演化研究
杨世兴,付玉华,占飞

Study on Post Peak Damage Evolution of Tailings Filling Body by Confining Pressure and Slurry Concentration
Shixing YANG,Yuhua FU,Fei ZHAN
表2 充填体试件特征参数
Table 2 Characteristic parameters of backfill specimen
试件编号料浆浓度/%E/MPaσP/MPaεP/εεu/εβADPB
Q-4-2661991.4010.01010.03292.30111 842.8690.30352.368
Q-4-3664151.9270.00680.03002.15314 719.3690.31749.519
Q-5-170700.8840.01600.03813.7441 121 237.1280.21170.403
Q-5-2702381.9530.01150.02992.49119 407.2410.28668.031
Q-5-3701861.6390.01090.03714.22036 699 402.5000.19262.987
Q-6-1741130.8560.00940.03493.3321 311 592.3780.23157.464
Q-6-2744612.6070.00780.02922.63799 620.2480.27560.326
Q-6-3743302.5070.00990.02853.299953 328.8340.23378.318