铝硅酸盐固废胶凝材料制备及其性能
叶智远,王倩倩

Preparation and Performance of Aluminosilicate Based Solid Waste Cemen-titious Materials
Zhiyuan YE,Qianqian WANG
表 2 原料的配合比设计
Table 2 Mixing design of the raw materials
样品编号RM∶CG煤矸石+赤泥/%熟料/%石膏/%石灰/%

S1

S2

S3

S4

S5

S6

S7

S8

S9

1∶9

2∶8

3∶7

4∶6

5∶5

6∶4

7∶3

8∶2

9∶1

65

65

65

65

65

65

65

65

65

15

15

15

15

15

15

15

15

15

10

10

10

10

10

10

10

10

10

10

10

10

10

10

10

10

10

10