表2 地球化学元素相关关系矩阵
|
Table 2 Correlation matrix of geochemical elements
|
|
相关系数 | Cu | Pb | Ni | Mn | Ag | Zn | Co | B | As | Sb | Bi | Hg | Au |
---|
Cu | 1 | - | - | - | - | - | - | - | - | - | - | - | - | Pb | 0.705 | 1 | - | - | - | - | - | - | - | - | - | - | - | Ni | 0.307 | -0.059 | 1 | - | - | - | - | - | - | - | - | - | - | Mn | 0.425 | 0.179 | 0.589 | 1 | - | - | - | - | - | - | - | - | - | Ag | 0.743 | 0.981 | 0.001 | 0.236 | 1 | - | - | - | - | - | - | - | - | Zn | 0.575 | 0.334 | 0.470 | 0.770 | 0.388 | 1 | - | - | - | - | - | - | - | Co | 0.359 | 0.004 | 0.767 | 0.835 | 0.064 | 0.666 | 1 | - | - | - | - | - | - | B | 0.034 | -0.003 | 0.187 | 0.154 | 0.045 | 0.149 | 0.165 | 1 | - | - | - | - | - | As | 0.439 | 0.486 | -0.022 | 0.163 | 0.527 | 0.290 | 0.047 | 0.035 | 1 | - | - | - | - | Sb | 0.694 | 0.989 | -0.013 | 0.227 | 0.975 | 0.372 | 0.055 | 0.021 | 0.466 | 1 | - | - | - | Bi | 0.233 | -0.010 | 0.311 | 0.27 | 0.051 | 0.295 | 0.280 | 0.128 | 0.160 | -0.010 | 1 | - | - | Hg | 0.161 | 0.222 | 0.034 | 0.137 | 0.221 | 0.163 | 0.102 | 0.078 | 0.117 | 0.227 | 0.002 | 1 | - | Au | 0.227 | 0.002 | 0.137 | 0.206 | 0.053 | 0.402 | 0.069 | -0.006 | 0.218 | 0.007 | 0.401 | 0.012 | 1 |
|
|
|