选冶联合处理低品位含金尾矿的试验研究
冯大伟,王玲

Experimental Research on Treatment of Low-grade Gold-bearing Tailings by Combined Process of Concentration and Smelting
Dawei FENG,Ling WANG
表7 开路试验结果
Table 7 Results of open circuit test
产品名称产率/%金品位/(g·t-1金回收率/%
精矿12.365.3077.07
精2尾0.812.842.71
精1尾4.121.406.63
扫1精5.761.006.78
扫2精3.990.361.69
尾矿72.960.065.12
原矿100.000.85100.00