含水率对重塑红黏土反复抗剪强度影响试验研究
林斌,田竹华,陈雨漫

Experimental Study on Effect of Water Content on Repeated Shear Strength of Remolded Red Clay
Bin LIN,Zhuhua TIAN,Yuman CHEN
表1 重塑红黏土试样反复直剪次数统计
Table 1 Statistics of repeated direct shear times of remolded red clay samples
含水率/%平行试样反复直剪次数/次
试样1试样2试样3试样4试样5试样6试样7试样8
15.054573454
18.044446445
19.545445543
21.044453544
24.043364444