表2 焦家金矿磨矿循环产品粒度组成
|
Table 2 Particle size composition of Jiaojia gold ore grinding cycle products
|
|
粒级/mm | 球磨机给矿 | 旋流器沉砂 | 旋流器溢流 | 球磨机排矿 |
---|
产率/% | 正累积产率/% | 产率/% | 正累积产率/% | 产率/% | 正累积产率/% | 产率/% | 正累积产率/% |
---|
合计 | 100.00 | - | 100.00 | - | 100.00 | - | 100.00 | - | +15.00 | 0.29 | 0.29 | - | - | - | - | - | - | 15.00~12.00 | 4.12 | 4.41 | 0.16 | 0.16 | - | - | - | - | 12.00~8.00 | 18.38 | 22.79 | 1.40 | 1.56 | - | - | 0.56 | 0.56 | 8.00~5.00 | 32.59 | 55.38 | 4.26 | 5.82 | - | - | 2.31 | 2.87 | 5.00~2.50 | 6.05 | 61.43 | 2.30 | 8.12 | - | - | 2.76 | 5.63 | 2.50~0.90 | 13.21 | 74.64 | 8.28 | 16.40 | 0.02 | 0.02 | 7.94 | 13.57 | 0.90~0.45 | 7.85 | 82.49 | 17.03 | 33.43 | 0.42 | 0.44 | 15.05 | 28.62 | 0.45~0.30 | 4.08 | 86.57 | 19.66 | 53.09 | 3.12 | 3.56 | 17.32 | 45.94 | 0.30~0.20 | 2.22 | 88.79 | 12.39 | 65.48 | 6.44 | 10.00 | 11.54 | 57.48 | 0.20~0.15 | 2.74 | 91.53 | 13.53 | 79.01 | 15.63 | 25.63 | 14.41 | 71.89 | 0.15~0.10 | 1.06 | 92.59 | 4.43 | 83.44 | 8.83 | 34.46 | 4.95 | 76.84 | 0.10~0.074 | 1.00 | 93.59 | 3.79 | 87.23 | 9.42 | 43.88 | 4.22 | 81.06 | 0.074~0.038 | 1.69 | 95.28 | 4.38 | 91.61 | 16.16 | 60.04 | 3.54 | 84.60 | 0.038~0.019 | 1.38 | 96.66 | 2.52 | 94.13 | 11.39 | 71.43 | 6.50 | 91.10 | 0.019~0.010 | 1.05 | 97.71 | 1.81 | 95.94 | 10.38 | 81.81 | 3.25 | 94.35 | -0.010 | 2.29 | 100.00 | 4.06 | 100.00 | 18.19 | 100.00 | 5.65 | 100.00 |
|
|
|