地聚合物混凝土配比及力学性能研究
|
丁琴,陶明,李响
|
Study on Proportion and Mechanical Properties of Geopolymer Concrete
|
Qin DING,Ming TAO,Xiang LI
|
|
表2 地聚合物胶砂试验配比
|
Table 2 Proportion of geopolymer mortar test
|
|
试验 编号 | 模数 | 碱掺量 /% | 一锅胶砂材料用量/g |
---|
粉煤灰 | 矿粉 | 碱激发剂 | 细骨料 | 水 |
---|
1 | 1.0 | 10 | 225.0 | 225.0 | 90.6 | 1 350.0 | 179.4 | 2 | 1.0 | 15 | 225.0 | 225.0 | 136.0 | 1 350.0 | 156.5 | 3 | 1.0 | 20 | 225.0 | 225.0 | 181.3 | 1 350.0 | 133.7 | 4 | 1.2 | 10 | 225.0 | 225.0 | 95.7 | 1 350.0 | 174.3 | 5 | 1.2 | 15 | 225.0 | 225.0 | 143.5 | 1 350.0 | 149.0 | 6 | 1.2 | 20 | 225.0 | 225.0 | 191.3 | 1 350.0 | 123.7 | 7 | 1.4 | 10 | 225.0 | 225.0 | 100.0 | 1 350.0 | 170.0 | 8 | 1.4 | 15 | 225.0 | 225.0 | 149.9 | 1 350.0 | 142.6 | 9 | 1.4 | 20 | 225.0 | 225.0 | 199.9 | 1 350.0 | 115.1 |
|
|
|